WELDING PROCEDURE SPECIFICATION EN15614-1 at NFK

🌍 International Standards – Foundation of Stable Quality

At NFK, we have established and implemented the Welding Procedure Specification (WPS) according to the EN ISO 15614-1:2004 standard. This is an important international benchmark, certified by Lloyd’s Register Energy Japan, to ensure that all NFK welding products achieve high reliability and consistency.

🔧 Main Content

  • Welding Process: TIG, without filler material, suitable for thin materials.
  • Material: SUS304, thickness of only 0.25 mm – requires precise welding techniques and strict heat control.
  • Preparation Method: Mechanical processing and surface cleaning to ensure the weld is free from contaminants.
  • Welding Parameters:
    • Current: 16–18 A
    • Voltage: 8–10 V
    • Travel Speed: 55–60 cm/min
    • Torch Angle: 85°
    • Gas Shielding: 99.9% pure Argon, flow rate of 7 L/min, combined with copper backing to stabilize the weld.
  • Inspection: Certified by Lloyd’s Register Energy Japan through WPQR (Welding Procedure Qualification Record), confirming the practical applicability of the procedure.

✅ Significance for Product Quality

Adhering to EN15614-1 brings core values to NFK:

  • Ensures uniform and stable welds even on thin materials.
  • Increases product reliability and lifespan, especially in high-demand industrial applications.
  • Affirms production capabilities to international standards, building strong trust with global customers.

📢 Message from NFK

NFK not only manufactures flexible hoses and custom welding products but also commits to stable quality through the application of WPS EN15614-1. This demonstrates a serious investment in technology and quality control, ensuring customers can confidently choose NFK products for the most demanding applications.

Click here for consultation on
Flexible Hose and Expansion Joint.

(+84) 221-3900-170Open hour 08:00AM - 16:45PM

Contact Us CHECKLIST